Diagnostics of hydrogen macrodelamination in the wall of pipe elbow of a natural gas transmission pipeline / Kharchenko, L. Ye., Kunta, O. Ye., Zvirko, O. I., Savula, R. S., Duriahina, Z. A. (2015)
Ukrainian

English  Materials Science (Physicochemical mechanics of materials)   /     Issue (2015, 51 (4))

Kharchenko L. Ye., Kunta O. Ye., Zvirko O. I., Savula R. S., Duriahina Z. A.
Diagnostics of hydrogen macrodelamination in the wall of pipe elbow of a natural gas transmission pipeline


Cite:
Kharchenko, L. Ye., Kunta, O. Ye., Zvirko, O. I., Savula, R. S., Duriahina, Z. A. (2015). Diagnostics of hydrogen macrodelamination in the wall of pipe elbow of a natural gas transmission pipeline. Materials Science (Physicochemical mechanics of materials), 51 (4), 84-90. http://jnas.nbuv.gov.ua/article/UJRN-0000664248 [In Ukrainian].

 

Institute of Information Technologies of VNLU


+38 (044) 525-36-24