Restoration of single crystal blades of gas turbines of high-temperature nickel alloys with surface defects and damages by surfacing / Jushchenko, K. A., Gakh, I. S., Zaderij, B. A., Zvjagintseva, A. V., Karasevskaja, O. P. (2019)
Ukrainian

English  Automatic Welding   /     Issue (2019, 6)

Jushchenko K. A., Gakh I. S., Zaderij B. A., Zvjagintseva A. V., Karasevskaja O. P.
Restoration of single crystal blades of gas turbines of high-temperature nickel alloys with surface defects and damages by surfacing


Cite:
Jushchenko, K. A., Gakh, I. S., Zaderij, B. A., Zvjagintseva, A. V., Karasevskaja, O. P. (2019). Restoration of single crystal blades of gas turbines of high-temperature nickel alloys with surface defects and damages by surfacing. Automatic Welding, 6, 21-28. http://jnas.nbuv.gov.ua/article/UJRN-0001003044 [In Russian].

 